Fibre-reinforced polymer (FRP) formwork refers to glass-fibre-reinforced polymer (GFRP) shells and profiles used either as temporary shuttering that is removed after the concrete has cured, or as permanent, stay-in-place (SIP) elements that remain bonded to the cast concrete as a structural part of the finished element. The two main production routes behind these systems are pultrusion, which produces straight box or profile sections, and laminated shell moulding.

In so-called lost-formwork applications, the GFRP shell is never removed — it becomes a permanent skin bonded to the concrete underneath. One documented SIP system illustrates how this works in practice: a moulded GFRP grating is adhesively bonded to square pultruded GFRP box sections, and the resulting cavity is then filled with concrete to create a composite floor slab. The grating does more than just hold the concrete in place while it sets — it also acts as a confinement layer that interacts mechanically with the cured material.

How Is the Concrete Mechanically Connected to the GFRP Shell? Holes are cut into the top flange of the pultruded box sections before casting. As concrete flows into these openings, it forms shear studs at the interface between the grating and the box sections once cured. During casting, GFRP dowels are additionally inserted through the assembly, creating a further mechanical key between grating and box section. Together, these two connection mechanisms are designed to transfer longitudinal shear across the composite cross-section without relying on adhesive bond alone.

What Does Confinement Do to the Concrete's Strength? A PhD thesis on this stay-in-place structural formwork system found that the GFRP grating, acting as confinement, increased both the ultimate strength and the strain capacity of the concrete compared with unconfined concrete. The reported shear connection between grating and box section showed elastic-plastic behaviour, which allowed longitudinal shear failure to develop progressively and in a controlled manner rather than suddenly.

Six slab specimens measuring 300 x 150 x 3000 mm were tested under five-point bending as part of the same research programme. All six were reported as exhibiting ductile failure behaviour — meaning the slabs deformed visibly and progressively before ultimate failure, rather than failing abruptly without warning.

For specifiers evaluating precast and composite floor elements, the confinement effect and ductile bending behaviour documented in this research are the two properties worth asking suppliers about directly: how much strength gain does the shell contribute over unconfined concrete, and what failure mode does the connection detail produce under load.